Determination of glass transition temperature and irradiation resistance of elastomeric materials based on chlorinated natural rubber
(RAD Association, 2018-06-18)
Synthetic rubbers have different surface structures but benefit from chlorination. In many cases their tensile strength and extensibility is lower than natural rubber and for that reason more easily mechanically damaged. ...
Effect of silica on the properties of elastomeric materials based on NR/BR/SBR ternary rubber blend
(University of Banja Luka, Faculty of Technology, Banja Luka, 2018-11-02)
The effects of pyrogeneous silica on the mechanical properties of elastomeric
materials based on natural rubber (NR), polybutadiene rubber (PB) and styrene butadiene
rubber (SBR) are reported. For sample preparations the ...
Effect of silica on the properties of elastomeric materials based on NR/BR/SBR ternary rubber blend
(University in Banjaluka, Faculty of Technology, 2018-11-02)
The effects of pyrogeneous silica on the mechanical properties of elastomeric materials based on natural rubber (NR), polybutadiene rubber (PB) and styrene-butadiene rubber (SBR) are reported. For sample preparations the ...
The influence of modification and the particle size of the montmorillonite on the hydrolytic stability of urea-formaldehyde composite
(Materials Research Society of Serbia, 2019-09-02)
Urea–formaldehyde (UF) resin adhesive is a polymeric condensation product of formaldehyde with urea and is considered as one of the most important wood adhesives. In spite of some advantages such as lower cost, fast curing, ...
The effect of UV irradiation on hydrolytic stability of urea-formaldehyde resins filled with thermally modified montmorillonite
(RAD Centre, Niš, Serbia, 2019-06-10)
The hydrolytic stability of organic-inorganic nano-composites prepared by a two-stage
polymerization of urea-formaldehyde resin (UF) filled with thermally activated montmorillonite (MMT) has been assessed before and after ...
Irradiation resistance of elastomeric composites based on NR/CSM blend and waste rubber powder
(RAD Centre, Niš, Serbia, 2021-06-14)
Effect of waste rubber particles (WTR) size on elastomers based on natural rubber and chlorosulfonated polyethylene rubber (NR/CSM= 50:50) was studied. Two types of WTR with different particle size (150–250 μm and 450–600μm) ...